LION 800 CONSTRUCTION PART 2

August 4-5
Finishing of the shell, priming

The hull is leveled with putty, the work is carried out in two stages, the first stage is coating with the putty of the whole hull of the yacht, after which a rough grinding with a hand tool is performed. The tool for grinding is easy to make by yourself. For this purpose, the length of the plywood is 1×0.2 meters, sandpaper is fixed on the bottom part, handles are fixed on the upper part at a convenient distance, this tool can grind large surfaces achieving very good quality.

After leveling the surface, a grout is applied, according to the technology specified by the manufacturer or in the painting scheme.

 

Tagged , , ,

2 thoughts on “LION 800 CONSTRUCTION PART 2

  1. how many layers of glass will you be doing?

    1. The yacht is covered with two layers of fiberglass with a density of 300 gr.m2